Poor adhesion
Release time£º2023.02.22    Source£ºShandong Little Bee New Material Co., Ltd   Number of visits£º
There are two types of poor adhesion

(1) Poor adhesion between paint films:

The direct cause is that there is no sanding between the coatings during spraying. Waterborne industrial paint is with the volatilization of water, physical filming, relying on the friction of the surface to improve adhesion. Goris has a water-based paint finish that can be sprayed without sanding primer, which will be introduced later;

The indirect reason is that the temperature is high in summer, and the interface between wet film and dry film is insufficient time for the formation of a firm layer, which makes the adhesion worse. Therefore, when spraying, it is appropriate to apply in the morning and evening to ensure the adhesion of the product.

(2) Poor adhesion between paint film and substrate:

This is similar to the cause of poor adhesion of oil-based paint, and there is no too much answer.
Next£ºWhy does the paint film "whiten"?I have a ceiling. There is no news£¡
About           honor           Products           News           Culture           Serve customers           notes           Contact          
Follow us
Welcome to Scan
Contact US About US Cooperative Unit
Consultation Hotline£º400-661-6377
Fax number£º273100
ADDRESS£ºNorth District of Qufu Economic Development Zone
About US
Qualifications
Industry news
China Building Materials
Shanghai Mitsubishi Elevator
Copyright 2006 - 2024  Shandong Little Bee New Material Co., Ltd£¨www.xmfsq.com£©  All Right Reserved.